AnswerMaterials
Why are PETG supports so hard to remove?
PETG bonds to itself, so its supports fuse across the default 0.2 mm gap. Raise Top Z distance 0.05 to 0.1 mm at a time, or print the interface in PLA at 0 mm.
AnswerMaterials
PETG bonds to itself, so its supports fuse across the default 0.2 mm gap. Raise Top Z distance 0.05 to 0.1 mm at a time, or print the interface in PLA at 0 mm.
AnswerMaterials
Print only the interface in a material that won't bond: PETG under PLA, PLA under PETG, ABS or ASA under nylon. Makers then allow a 0 mm top Z distance.
AnswerMaterials
Shipped PETG profiles retract 0.4 to 1 mm at 30 to 45 mm/s on direct-drive printers and 2.5 to 8 mm on Bowden printers, close to each printer's PLA values.
AnswerTroubleshooting
Pull or cut the loose strings, then hit the fine wisps with a heat gun at about 200 °C for one or two seconds. Longer can deform PLA, which softens at 54 to 60 °C.
AnswerTroubleshooting
Shipped profiles run PETG 20 to 35 °C hotter than PLA, and its melt draws out into threads. Dry it, drop the nozzle 5 to 10 °C, and expect a few fine hairs.
AnswerHardware
Yes. Copy the 3/4-11.5 NH garden hose thread, not 3/4 in NPT, let a rubber washer seal a flat face, and print PETG or ASA upright with four or more walls.
AnswerMaterials
No. Data sheets list PLA, PETG, ABS, ASA, nylon and TPU as insoluble in water. Only PVA and BVOH support filaments dissolve, in a few hours to overnight.
AnswerMaterials
A closed print with sparse infill usually floats. Solid PLA (1.24 g/cm³), PETG, ABS and nylon sink in water (1.00 g/cm³); polypropylene (0.9 g/cm³) floats.
AnswerMaterials
Brush a cured coat of XTC-3D epoxy over the cavity, then the release agent your casting maker names. Test platinum silicone on a sealed scrap: it can stay tacky.
AnswerMaterials
Coat it in an epoxy its maker rates safe near reptiles and cure it fully. Bearded dragons bask at up to 42 °C (108 °F) and PLA softens at 57 °C: use PETG or ASA there.
AnswerMaterials
UV printer resin brushed on hardens only where 405 nm light or sunlight lands, and no maker documents it as a sealant. Uncured, it carries H317 (skin allergy).
AnswerMaterials
Yes for seams and joints, not as a coat: silicone sealant is not paintable, goes on at least 1/8 in (3.2 mm) thick and is water ready in 30 minutes to 12 hours.
AnswerMaterials
Let the paint dry (72 hours to two weeks for Liquitex acrylics), then brush or spray two or three thin clear coats. Keep to each maker's recoat time.
AnswerHardware
Print the hull with 4 perimeters (2 in ASA), brush epoxy inside and out, grease the stuffing tube, seal the rudder and hatch, then float-test it overnight.
AnswerMaterials
A moderate fan, about 20 to 60%, not PLA's 100%. Prusa's PETG profile runs 30 to 50%, Bambu's 20 to 40%; both keep it off for 3 layers, more for bridges.
AnswerMaterials
Mostly no: at the maker's temperature, no maker names harm from extra hours for PLA or PETG. Heat above it fuses coils; nylon and PC can turn brittle.
AnswerMaterials
Usually not from an intact vacuum bag. Dry PETG once an opened spool has sat out or pops: Bambu Lab's line is 72 hours in air above 50% RH.
AnswerHardware
Only the Bambu Lab AMS 2 Pro (up to 65 °C) and AMS HT (up to 85 °C) dry filament. The original AMS and AMS lite don't heat. AMS 2 Pro PETG preset: 65 °C, 12 h.
AnswerMaterials
Yes for PLA, PETG and TPU: Nesco, COSORI and Presto dehydrators reach 71 to 74 °C. Not for nylon or PC, which need 75 to 90 °C. Lift the trays out to fit the spool.
AnswerMaterials
Only if the oven holds the drying temperature. GE's Warm mode bakes at 170 °F (77 °C), past PLA's 60 °C glass transition. Bambu Lab says no; Prusa allows one.
AnswerMaterials
Yes, on dryers built for it. Bambu Lab's AMS 2 Pro and AMS HT drop to 45 °C with PLA and 55 °C with PETG once a print starts; standalone dryers hold their setting.
AnswerMaterials
Yes, at the PLA's setting only. Makers dry PLA at 45 to 55 °C and PETG at 55 to 65 °C, so the ranges meet only at 55 °C, Prusa's 6-hour PETG setting.
AnswerMaterials
Dry PLA at 45 to 55 °C, PETG at 55 to 65 °C, TPU at 60 to 70 °C and nylon at 75 to 100 °C, for 4 to 12 hours, per Bambu Lab, Prusa and Polymaker.
AnswerTroubleshooting
Once the spool is dry, stringing comes from settings: Prusa says lower the nozzle 5 to 10 °C, Bambu Lab adds retraction up to 2 mm and shorter travel.
AnswerMaterials
Heat the spool below its softening point, then seal it with desiccant. Bambu Lab's oven setting is 50 °C for PLA and 60 to 65 °C for PETG, for 8 hours.
AnswerTroubleshooting
Wet filament pops or hisses at the nozzle, bubbles, strings and prints rough. To confirm, dry it (PLA 50 °C, PETG 60 to 65 °C, 8 hours) and reprint.
AnswerMaterials
Dry PETG at 55 to 65 °C (131 to 149 °F) for 6 to 8 hours. Prusa sets 55 °C, Bambu Lab 65 °C, Polymaker 60 to 65 °C. None of them goes above 65 °C.
AnswerMaterials
Seal it in an airtight bag or box with desiccant below 20% RH, Bambu Lab's target for PLA, PETG, TPU, PC and nylon. Room air can re-wet it in 2 to 12 hours.
AnswerTroubleshooting
Bambu Lab's X1C and P1S guides load PLA at 220 to 230 °C and pull at 70 to 100 °C; the H2D, H2S and P2S run it from Toolbox > Nozzle Cold Pull Maintenance.
AnswerTroubleshooting
Yes, up to a point: Prusa adds 5 to 10 °C when a material won't stick, but makers stop near the glass transition, 61 °C for PLA and 81 °C for PETG.
AnswerTroubleshooting
Let it cool: Prusa waits for room temperature and Bambu Lab for 35 °C or lower on textured PEI. On Bambu's SuperTack plate, reheat a stuck print to about 50 °C.
AnswerTroubleshooting
The first layers stay soft and squash out into elephant foot; Polymaker caps PLA at 60 °C. Too hot also clogs nozzles and bonds PETG hard enough to tear PEI.
AnswerTroubleshooting
Yes. In a 2021 ABS test, corner lift was lowest at a 90 °C bed, 0.89 mm, and grew both cooler and hotter: 1.65 mm at 80 °C, 1.37 mm at 100 °C.
AnswerTroubleshooting
No filament comes out, lines print thin with gaps, the extruder clicks, or a purged strand curls back onto the nozzle. Prusa tests it at 260 °C for PLA.
AnswerTroubleshooting
TPU is too soft to push old filament out of the nozzle. Bambu Lab says cold pull with PLA or PETG first: flush at 250 °C, pull PLA at 70 to 100 °C.
AnswerMaterials
Prusa's tests found PLA works best for a cold pull, at 85 to 100 °C. Bambu Lab adds PETG for high-flow nozzles; Creality favors nylon at 140 to 160 °C.
AnswerTroubleshooting
Pull PLA at 70 to 100 °C after heating to 200 to 270 °C. UltiMaker pulls ABS and cleaning filament at 140 to 160 °C; Creality gives 120 °C for PETG.
AnswerMaterials
Bambu Lab's heated-bed drying table sets 60 to 70 °C for PLA, 75 to 85 °C for PETG and 80 to 90 °C for TPU, for 12 hours, spool covered and printer closed.
AnswerTroubleshooting
A blockage makes the motor skip steps. Check for a nozzle clog, then first layer height, heat creep, speed (8 to 12 mm³/s on an all-metal hotend) and the gears.
AnswerTroubleshooting
Heat the hotend to 260 °C after PLA or 280 °C after PETG, push a 1.5 mm rigid wire down from the top, or pull the stub up hot with pliers.
AnswerTroubleshooting
Most slicer defaults use one bed temperature for all layers. PrusaSlicer starts PETG at 85 °C then 90 °C; OrcaSlicer starts ABS at 105 °C then 100 °C.
AnswerTroubleshooting
Clear the jam at 250 °C, cold pull from 220 to 100 °C, then cut the heat: hotend fan always on, door open for PLA on a 45 °C+ bed, retraction 2 mm or less.
AnswerTroubleshooting
A 0.3 to 0.35 mm needle, the size Prusa Research bundles, pushed 1 to 2 cm up from below with the nozzle hot. It must be thinner than the 0.4 mm bore.
AnswerMaterials
About 70 to 80 °C. Bambu Lab lists 60 to 80 °C for all its PETG, Prusa runs 85 then 90 °C. Put glue stick on smooth PEI or glass first.
AnswerTroubleshooting
PETG residue stays in the hotend when PLA goes in at 190 to 230 °C. Load the PLA at the PETG temperature, 230 to 260 °C, so it pushes the old plastic out.
AnswerTroubleshooting
Heat the nozzle to 260 °C for PLA or 280 °C for PETG and push filament through, then use a 0.3 to 0.35 mm needle, a cold pull, and finally a nozzle swap.
AnswerTroubleshooting
Bambu Lab's guides heat the nozzle to 250 °C for PLA, run the included pin up and down in the tip, then cold pull. If the clog survives that, swap the hotend.
AnswerMaterials
Yes: Bambu Lab says damp nylon, PC and fiber-filled filament are prone to clogging. Wet PLA mostly bubbles and strings. Dry PLA at 45 to 55 °C for 6 to 8 hours.
AnswerHardware
Yes for bin clips, shelf supports and drawer rails at 40 °F (4 °C). PETG or ABS beats PLA on impact. Gaskets, sealed-system, electrical and water-line parts stay OEM.
AnswerMaterials
Manufacturer HDT and Tg figures for PLA, PETG, ABS, ASA, nylon, PC and PP set against the 150 °F dishwasher sanitize rinse, with margins in °C.
AnswerTroubleshooting
Thin-walled ones do. Prusa's PLA flower pots held water; its tests needed 4 perimeters for PLA and PETG and 5+ bottom layers. Seal the inside or print a saucer.
AnswerMaterials
Coat the print in a sealant its maker calls fish safe once cured, such as Pond Armor Pond Shield (24 hours to cure), and use natural PLA or PETG with no added color.
AnswerMaterials
Iron temperature per material for heat-set inserts: about 225 °C for PLA, 245 °C for PETG and 265 °C for ABS, from CNC Kitchen's printing temperature plus 10 to 20 °C.
AnswerHardware
In CNC Kitchen's M3 test in PETG, a Helicoil and a heat-set insert pulled out at the same load, but the Helicoil stripped at 1 Nm against 3 Nm for the insert.
AnswerMaterials
PETG is insoluble and takes up 0.45% water at saturation, about the same as PLA. Prints leak at the seams: Prusa needed 4 perimeters before PETG held water.
AnswerHardware
Print ASA or PETG with 2 to 3 mm walls, seal the lid with an O-ring at 20 to 30 percent squeeze under screws, use IP68 cable glands and a vent, then test.
AnswerHardware
A numbered gear recipe (material, teeth, perimeters, infill, orientation) plus the 2022 Polymers wear test where PETG gears outlasted PLA by 22.3 percent and ABS by 37.
AnswerHardware
Published pressure results for printed parts: Prusa Research's 20 and 30 meter dives, a forum test at 5 to 8 bar, and the O-ring rule for threaded fittings.
AnswerMaterials
A decision table from what the broken part faces (heat, sun, load, chemicals) to a material class, with HDT, impact and absorption figures from manufacturer data sheets.
AnswerHardware
Not for PLA, PETG or TPU. Prusa requires a glue stick for ABS, ASA, nylon and PC Blend on textured PEI, and Bambu Lab says those four may need one.
AnswerHardware
CNC Kitchen's M3 test in PETG: a bottom-pocket nut held 166 kg against 119 kg for a heat-set insert, but the insert took more torque. When each fastening wins.
AnswerMaterials
PLA, PETG, ASA, PP and PC compared for holding water: the perimeter count Prusa needed, data-sheet water absorption, heat limits and outdoor use.
AnswerHardware
Yes: brass heat-set inserts hold in PETG at an iron temperature of about 245 °C, and the part stays rigid to a glass transition near 80 °C. Expect stringing from the tip.